In the vacuum salt-making system, its raw material is brine, which contains a large number of corrosive media. Its main equipment, such as brine preheater, heater, evaporation tank at higher temperatures for a long time in contact with high concentrations of brine, constantly subject to the impact of salt and sand, under these conditions, the equipment to operate normally for a long time, corrosion is a key issue.

There are many reasons for corrosion, among which the presence of O2, high temperature, Cl- and solid salt scouring are the main factors. Commonly used anti-corrosion methods are deoxygenation, pH adjustment, electrochemical protection, coating protection, the use of anti-corrosion materials. The use of anti-corrosion materials is a very effective way to prevent corrosion, titanium and titanium alloy in the vacuum salt application is one of the examples.
Preheater
Raw materials need to be preheated before entering the heater to save energy. Preheaters used to be often tube heat exchanger, heat pipe material made of carbon steel, very easy to clog, corrosion through the tube, often to replace the heat pipe, shutdown maintenance, which brings great inconvenience to the production. There is also the use of copper tube preheater, corrosion still exists, the service life is extended to 1 year, but still very short, and copper tube cost is higher.
Until the emergence of titanium plate heat exchanger. Plate heat exchanger heat transfer surface for the plate, the strength is not as good as the tube heat exchanger, but its heat transfer is good, less material, light weight, easy to maintain, its life expectancy of up to 15 years. Such as Zigong Ziliujing salt plant using pure titanium plate heat exchanger from 1994 to date, the titanium plate is still bright as new, has never been replaced, the economic benefits are obvious.

Heater
Due to the heater heat exchanger tube dense row in the tube plate, so the maintenance is quite time-consuming, every year all need to replace the heating tube once. Ⅱ effect, Ⅲ effect temperature is lower, the heating tube can be used for about 2 years. Ⅳ effect temperature can only be used for a minimum of 4 years on the need for replacement, overhaul downtime delays in production, yield reduction, production is seriously affected, and maintenance costs are high (some manufacturers will be used in the heating chamber of copper, the situation has improved, but Ⅰ effect of the use of life is only 3-5 years). In view of the characteristics of titanium, if titanium is used in the heater, the situation will be greatly improved.